Andy Coates looks at the fundamentals of working with burrs

Burred wood, or ‘burl’ in the US, is indisputably attractive, and the burr form of any wood species seems to offer an enhanced version of the plain material. As such it is highly desirable for woodturners. There are, however, a number of potential issues with using burr, but before we look at them, we need to look at what burr is.
The truth is that there is no single definitive answer as to what a burr is. There are a number of possible causes for the anomaly, and a burr may be the result of one or any combination of factors, ranging from faulty genetic code through to a survival response of the tree to a viral, fungal or other attack such as insect infestation. The tree’s response to any combination of these factors is to produce burr. Usually seen as an extending ‘growth’ on the outside of the tree’s trunk or branches – but also often found on the root ball below the surface of the soil. This is often the highest quality burr – burr is the direct result of hundreds if not thousands of potential, or dormant, branches all trying to grow from the same restricted area of the tree. These branches never come to fruition, although commonly will form tiny branchlets that may even produce leaves. In extreme and rarer cases, the burr may even extend through the whole of the trunk of the tree.
When these burrs are cut parallel to the tree the surface revealed is covered in tiny ‘pips’, wild grain and usually dramatic colours, and this is what turners find so attractive and desirable – but this figuring comes at a price. For the purposes of illustrating the process I turned a small platter from a blank cut from a board of burr elm (Ulmus procera).


Basic tools and equipment
Working burr does not require any specialist tools and can be achieved with a very basic set comprising those detailed right. Always keep in mind that tools need to be kept sharp to achieve the cleanest cuts. You may need to re-grind more frequently than for non-burred wood of the same species. You may also find, with some species, that the scraper works better in certain circumstances.

Burr stock
Burred wood can be found via all the usual sources: timber mills, local supply through tree surgeons and from usual turning blank suppliers. Burr may be supplied in plank form, usually cut through and through, in complete whole burr form, which can range in size from small burrs to dining table-size burrs, and as part of a whole trunk, leaving the machining choices to the purchaser. Buying a whole trunk, either burred through or merely containing extending burrs, may not be practicable for most turners, so buying individual burrs or boards may be the best route to turning burr. Burr in this format is usually more manageable, especially for novices, and if care is taken at selection you can ensure that no further dimensioning is required in order to mount on the lathe. Before you begin it is worth considering some of the potential pitfalls of working with burr. Exotic species of burr are also available and are highly sought after.




Potential problems
• Loose bark
• Embedded stones, grit, foreign objects, dirt
• Voids
• Irregular surface leading to holes forming in vessels
• Areas of very hard to very soft wood
• Highly variable grain direction
• May initially be out of balance
If the burr is from rootstock there is a high likelihood of embedded stones and grit that not only present an issue for tool edges, but also as a potential airborne hazard if they are ejected during turning. Blanks should be very carefully examined for embedded objects and cleaned carefully prior to working with them. Large burrs obtained freshly felled can be jet-washed to remove dirt, grit and stones, but a thorough visual inspection afterwards is still required. Embedded metal can also be an issue – barbed wire, bullets, nails, horseshoes and other metal are not uncommon. A cheap metal detector is a useful piece of equipment to have available for such situations.
Loose bark can present an airborne hazard, so careful inspection and removal with a pick are vital preparatory steps. Do not worry about ‘ruining the blank’, your safety is more important than the look of the surface of the blank. The irregular surface of burrs which have the bark retained gives rise to what are both a potential hazard and a potential feature: voids and breakthroughs. Many turners work to include voids in the finished objects, considering them desirable aesthetic features, but for the novice turner this can present a hazard and a difficulty. A void opening up means that there is an area of weakness in the object being turned, which, under stress, could cause the piece to fail during turning, so if voids appear, extra care should be taken.
The nature of burrs means that while on the tree there may have been water and debris collected in pockets which can lead to disease or insect activity resulting in punky, or rotten, areas in the wood. This can lead to the wood having hard and soft areas, which is always a problem, and some techniques are required to overcome them. We will discuss these later on.
Affordable stock
Burrs are often sold by price-per-unit weight, which can be costly if the burrs are on the large side. Board stock provides a more economical route into turning burred wood. Boards can be found in a range of thicknesses, but 25mm, 40mm and 75mm are quite common. Obviously, the thinner boards are cheaper, but how can we mount them? Firstly, scribe and cut a disc from the board. I cut one from a 35mm board at 210mm diameter.
The screw chuck might seem a logical solution, but on a board below 50mm thickness the hold is not ideal and this also presents design limitations. In order to maximise the wood available to turn, a glue chuck offers the best option.
A scrap block of wood is turned with a tenon on one side and a flat surface on the other. The glue chuck is then glued to a disc of burr elm and clamped until cured. With modern glues this can be as little as 15-30 minutes. The blank is then ready to be mounted and turned without wasting any of the expensive wood.


Cross section of glue chuck

Safety
Turning any wood, especially burrs, can be hazardous. You really do need to use PPE & RPE (personal and respiratory protective equipment) for any turning. There is a genuine risk from flying pieces of bark, detritus, stones and, in extreme cases, pieces of the vessel itself if unidentified flaws become evident later on. Learn to listen to the sound of the tool on the wood – often this will provide the first indication of a potential problem as the note changes. If you are concerned, stop the lathe and examine the workpiece. Are there voids? Are there cracks or fissures opining up? Is there some debris that the tool is catching? If the answer to any of these questions is yes, then you need to either deal with the issue so that it is safe to continue turning, or discard the workpiece as unsafe. An unresolved risk is a bad risk. Don’t take it.
Turning burr wood
Turning burr is essentially no different to turning ordinary wood. Tools need to be as sharp as possible, and bevel control needs to be firm but not aggressively so. The pips of burr are essentially small patches of end grain surrounded by side grain, so if the bevel is pushed too heavily into the surface of the wood the tool will bounce on the burr leading to a poor finished surface. Take controlled cuts with medium bevel pressure. True up the edge and face of the blank to try to improve balance and then mark and turn a recess appropriate for your scroll chuck. Marking the centre of the recess with the revolving ring centre provides an accurate reference point for reverse turning later. As an aid to producing the best shape it is helpful to true up the first 20mm or so of the front face of the blank. Along with a mark at the edge of the foot of the object this provides a reference for the shape you turn on the underside of the object. Once the outer shape has been completed the platter can be mounted on the tenon of the glue chuck and the interior turned. Remember that burr wood may not have as much strength as non-burred wood, and consequently may require a thicker profile for strength. To remove the glue chuck, reverse turning on a jam chuck or in Cole jaws is required. Apply appropriate pressure from the tailstock for a more than usually fragile workpiece.
When abrading burred wood extra care should be taken – abrasives can snag and catch in the fissures, so abrading with an arbor held at a sheer angle is possibly the safest method. Apply light pressure and let the abrasive do the work. This also helps to prevent differential abrading between hard and soft areas. It is not uncommon for a burr piece to require some hand abrading in order to complete the process.




Problems with turning burr
One of the main problems with turning burr is the wild grain, which can almost be like turning wood with no discernible grain direction. Although this is not strictly the case, the grain is almost certain to run in just about any direction as the wood grain runs around branchlets. This can result in the softer grain getting quite badly torn, even with a freshly sharpened tool. This problem is aggravated because the bevel is prone to bounce on the pips of end grain, but this can be controlled by ensuring bevel pressure is at the minimum.
You may find that, despite your best efforts, the finished surface is still poorer than you would hope for. Often the best solution (on the exterior shape) is to sheer cut on the wing of a long ground bowl gouge and then sheer scrape using a freshly sharpened scraper. A teardrop scraper works well for this purpose and is ideal for the interior of the platter. Abrasion may need to begin at 80-120, but a perfect surface is possible with care.
If it proves impossible to deal with the softer areas, a liberal coat of cellulose sealer will stiffen the fibres prior to sheer cutting or scraping. Allow the sealer to fully dry prior to continuing work.
When the piece is finished you must vacuum all the abrading dust from the fissures before sealing and finishing. Oil is a better finish than wax for burr, as wax will fill the fissures and look unsightly.



Making the most of burr material
Burr can be an expensive material, and as ever it is prudent to make the most of it. More advanced turners may consider taking rings from areas that would otherwise end up as shavings, or cores from the middle of bowls from about 150mm diameter. (Coring will be discussed in depth in a later article in the magazine.) Developing the habit of salvaging whatever you can is both sensible and satisfying. Having a small stockpile of useful additional material for inlays and features in future objects makes the effort worthwhile, and essentially they are free material. More importantly they are more useful than shavings.


Tips
Freshly felled, unseasoned (or green) wood, is far easier to turn in general, and this is equally true for burr stock. However, as burr dries out it has a tendency to pucker, or wrinkle, around the pips of end grain branchlets. Personally I find this quite an attractive feature, but many do not, and it may be frowned upon in a finished piece. If this concerns you then rough turning and allowing the workpiece to dry prior to final turning is the best option. Remember to leave the rough turned object at least 10% oversize to allow for warping. However, burr stock tends not to warp in the same predictable way that non-burred wood does, so be prepared by leaving the walls thicker than usual.
Grain direction
It is often stated that burr has no grain direction, and while turning burr may give this impression it isn’t strictly true. Burr might better be described as having potentially very wild grain. However, if the burr is cut parallel or perpendicular to the trunk there can be a distinct grain-like figure, and where this is apparent the usual rules about cutting with the grain should be followed wherever possible.
The appearance of both kinds of feature might also indicate the orientation of the workpiece for turning. For instance, would the burr look better on the top or the side of a box? Because of the nature of burr this is an option you do not usually have with conventional blanks. Turning may prove slightly more difficult than usual, but that should not stop you trying if you feel it will benefit the outcome.